发明名称 PAINT MATERIAL FOR INTERIOR THIN-PAINTING FINISH HAVING HUMIDITY ADJUSTMENT PERFORMANCE, MANUFACTURING METHOD THEREFOR, WALL MATERIAL FOR INTERIOR THIN-PAINTING FINISH HAVING HUMIDITY ADJUSTMENT PERFORMANCE, AND EXECUTING METHOD THEREFOR
摘要 PROBLEM TO BE SOLVED: To provide a paint material for an interior thin-painting finish having humidity adjustment performance which has crack resistance, adhesion strength, water-retainability, wear resitance, fading-proof performance, moisture absorbing/desorbing performance, and minus ion generating effect, a manufacturing method therefor, a wall material for an interior thin-painting finish having humidity adjustment performance, and an executing method therefor. SOLUTION: The paint material for the interior thin-painting finish having humidity adjustment performance contains 3 to 7 wt.% of white sand or white sand balloon, 2 to 10 wt.% of re-emulsification-type water-soluble resin, 5 to 40 wt.% of inorganic powder, 10 to 75 wt.% of aggregate, 0.5 to 10 wt.% of thickener, and 1 to 3 wt.% of organic fiber. COPYRIGHT: (C)2008,JPO&INPIT
申请公布号 JP2008101436(A) 申请公布日期 2008.05.01
申请号 JP20060286626 申请日期 2006.10.20
申请人 FUJIKAWA KENZAI KOGYO KK 发明人 HARADA SUSUMU;KOJIMA SHUSUKE;MORIMOTO MIKIKO
分类号 E04F13/02;C04B14/10;C04B14/16;C04B14/28;C04B16/06;C04B24/38;C04B28/12;C09D5/02;C09D7/12;C09D201/00 主分类号 E04F13/02
代理机构 代理人
主权项
地址