A method for producing toilet tissue is provided to maximize the efficiency of a functional additive material, by directly coating the functional additive material between a first web and a second web of the toilet tissue while producing the toilet tissue. A functional material is mixed into an adhesive agent(S41). A viscosity of the mixed matter of the functional material and the adhesive agent is regulated(S42). The mixed matter is inputted between a first web and a second web, and then the first web and the second web are bonded to each other, thereby preparing toilet tissue where the functional material is coated between the first web and the second web(S47). Further, the functional material is one of propolis, biotree, catechin, charcoal or herb. |