摘要 The invention relates to a method for recovering gold from an intermediate product or residue containing sulphur and iron generated in the leaching of a sulphidic raw material. The recovery of gold and the other valuable metals in the raw material takes place in a chloride environment. The gold contained in the intermediate product or residue is leached with divalent copper and chlorine in a copper (II) chloride-sodium chloride solution in conditions where the oxidation-reduction potential is in the range of 650-750 mV and the pH between 1 and 1.6. The acid generated during the feed of chlorine is neutralized with a suitable alkali. Neutralization avoids the costs of dissolving the iron.
申请公布号 US2007245856(A1) 申请公布日期 2007.10.25
申请号 US20050579092 申请日期 2005.04.25
申请人 OUTOKUMPU TECHNOLOGY OYJ 发明人 HAMALAINEN MATTI;HYVARINEN OLLI
分类号 C22B9/00;C22B;C22B3/10;C22B11/00;C22B11/06 主分类号 C22B9/00