摘要 |
A pavement using waste wood fiber and a paving method thereof are provided to prevent the surface temperature from rising, and to increase elasticity and permeability by laminating a grinded waste wood fiber layer, a cleaning waste wood fiber layer, and an elastic rubber chip layer. A pavement using waste wood fiber is constituted by laminating a grinded waste wood fiber layer(10) as a base layer which contains a compound of 100 wt% of the grinded waste wood fiber obtained by grinding the waste wood board and 20 to 40 wt% of the binder, a cleaning waste wood fiber layer(20) containing a compound of 100 wt% of the cleaning waste wood fiber obtained by cleaning the waste wood fiber and 80 to 120 wt% of the binder, and an elastic rubber chip layer made by compounding 20 to 35 wt% of the binder to the 100 wt% of the rubber chip of 1 to 5mm. |