摘要 |
<P>PROBLEM TO BE SOLVED: To provide an electroconductive anti-reflection laminate which does not cause interfacial debonding, even when the numbers of times of reciprocation of steel wool are increased in the scratch resistance test using steel wool. <P>SOLUTION: The electroconductive anti-reflection laminate is composed at least of a hardcoat layer, a metallic thin film layer and a transparent thin film layer laminated on a substrate. The hard coat layer has a hardness of ≥4H under a load of 500 g in the pencil hardness test and show an elastic deformation (the load curve and unload curve are identical within a 20% deviation) at a depth of indentation of ≤50 nm in the indentation test specified by JIS K 5600. <P>COPYRIGHT: (C)2007,JPO&INPIT |