Method of manufacturing a disguishing net used in order to conceal arms and vehicles from enemies consisted of three processes; at the first process the resin adhesion rate became about 180% with heating in the pin tenter knife coating M/C at 135± 3≦̸C for 2 min., at the second process the resin adhesion rate of disguising tape bacame about 160% with heating at 150±5≦̸C for 2-3min., at the third process the net and the tape was banded with a resin ring and a nipper.
|