发明名称 |
METHOD OF MANUFACTURING ANISOTROPIC OPTICAL FILM, ANISOTROPIC OPTICAL FILM, AND OPTICAL ELEMENT |
摘要 |
<P>PROBLEM TO BE SOLVED: To obtain an anisotropic optical film which has a high dichroic ratio without any optical defects, and also has an alignment direction different from a coating direction even while coating a base material almost in parallel to the subsreate (in a direction almost matched with a longitudinal direction or a lateral direction of the base material). <P>SOLUTION: When the film of an anisotropic optical material is formed by a wet film-forming method using the composition for forming the optical film, an alignment treatment direction of a substrate of the base material 10 is made to be an angle between 89° and 1° from the base material and the composition for forming the optical film is applied by moving a slot die 11 being an applicator almost in parallel to a base material direction of the base material 10. Thereby the anisotropic optical film which has alignment with an angle between 85° and 5° from the alignment treatment direction of the base material, is obtained. <P>COPYRIGHT: (C)2007,JPO&INPIT |
申请公布号 |
JP2007127897(A) |
申请公布日期 |
2007.05.24 |
申请号 |
JP20050321432 |
申请日期 |
2005.11.04 |
申请人 |
MITSUBISHI CHEMICALS CORP |
发明人 |
FUJIWARA TAKESHI;YAMAUCHI YASUTSUGU |
分类号 |
G02B5/30;G02F1/1335;G02F1/13363 |
主分类号 |
G02B5/30 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|