发明名称 |
METHOD FOR THERMAL STRENGTHENING OF STEEL GRINDING BALLS |
摘要 |
The invention relates to ferrous metallurgy. A method for thermal strengthening of steel grinding balls comprises the subcooling of balls after rolling on still air, quenching them to the reception of initial temperature of self-tempering, which exceeds at 50-80 °С the point of martensite transformations, and self-tempering which is carried out during not less than 50 hours with the rate of cooling of not more than 3 °С/h. A method allows the obtaining of steel balls with high mechanical properties and reducing a formation of cracks at quenching. |
申请公布号 |
UA82632(C2) |
申请公布日期 |
2008.04.25 |
申请号 |
UA20070005311 |
申请日期 |
2007.05.15 |
申请人 |
YEFREMENKO VASYL HEORHIOVYCH;TKACHENKO FEDIR KOSTIANTYNOVYCH;YEFREMENKO OLEKSII VASYLIOVYCH;PRYAZOVSK STATE TECHNICAL UNIVERSITY |
发明人 |
YEFREMENKO VASYL HEORHIOVYCH;TKACHENKO FEDIR KOSTIANTYNOVYCH;YEFREMENKO OLEKSII VASYLIOVYCH |
分类号 |
C21D9/36 |
主分类号 |
C21D9/36 |