摘要 |
PROBLEM TO BE SOLVED: To reduce the number of times of baking an AC-type plasma display panel. SOLUTION: At the manufacture of the back plate of the plasma display panel having a plurality of address electrodes and a dielectric layer covering the address electrodes, and barrier ribs in row and column directions formed on the dielectric layer, demarcating a discharging space in a row and a column at every cell, a pattern of the address electrodes is formed on a substrate by using metal paste containing crystallized glass, a layer of low melting point glass serving as the dielectric layer is formed on the pattern of the address electrodes, and further, the pattern of the barrier ribs in the row and column directions is formed on the low melting point glass layer for the dielectric layer by using the low melting point glass, and a black material layer containing crystallized glass is formed between adjacent barrier rib patterns in a row direction corresponding to a part laid between rows of the address electrode pattern. Afterwards, a lamination body of the address electrodes, the dielectric layer, the barrier ribs, and the black material layer is formed on the substrate by baking the address electrode pattern, the low melting point glass layer, the barrier rib pattern and the black material layer, simultaneously. COPYRIGHT: (C)2007,JPO&INPIT
|