摘要 |
<p>Provided is a preparation method of environment-friendly artificial landfill cover materials using industrial by-products such as sewage sludge, waste plaster, and waste silica to thus prevent waste in resources and environment contamination. The preparation method of artificial landfill cover materials comprises the steps of: mixing 100 wt% of sewage sludge and 5-30 wt% of quicklime for solidifying the sewage sludge; adding a porous deodorant at an amount of 10-50% by weight of 100% of the sewage sludge; and adding a mixture of waste plaster and waste silica mixed at a ratio of 1:0.7 to the sewage sludge solid at an amount of 10-30% by weight of 100% of the sewage sludge. The deodorant is used to remove ammonia gas generated during use of the quicklime.</p> |