摘要 |
PROBLEM TO BE SOLVED: To obtain a lubrication coating film composition that is obtained by using a thermosetting resin not restricted from an environmental problem and made into a coating film by heating at a relatively low temperature and has low friction, low abrasion and excellent corrosion resistance. SOLUTION: The lubrication coating film composition is obtained by dispersing either or both of furfural and furfuryl alcohol as a starting substance, a furan resin initial condensate to become a low-friction furan resin by curing and three kinds of solid lubricants of molybdenum disulfide, a polytetrafluoroethylene and graphite into an organic solvent. The amount of the furan resin initial condensate is preferably 30-65 wt.% of the whole composition. COPYRIGHT: (C)2007,JPO&INPIT |