发明名称 |
Method for making float glass having reduced defect density |
摘要 |
A method for reducing the defect density of glass comprising melting a glass composition comprising from 65-75 wt. % of SiO<SUB>2</SUB>; from 10-20 wt. % of Na<SUB>2</SUB>O; from 5-15 wt. % of CaO; from 0-5 wt. % of MgO; from 0-5 wt. % of Al<SUB>2</SUB>O<SUB>3</SUB>; from 0-5 wt. % of K<SUB>2</SUB>O; from 0-2 wt. % Fe<SUB>2</SUB>O<SUB>3</SUB>; and from 0-2 % FeO, wherein the glass composition has a total field strength index of greater than or equal to 1.23 is disclosed.
|