发明名称 |
Method for producing magnetostrictive element and sintering method |
摘要 |
In the step of sintering a compact that is finally to be a magnetostrictive element, when the temperature in a furnace is elevated, the atmosphere in the furnace is evacuated by a vacuum pump to keep the pressure in the furnace at negative pressure in a temperature range that allows thermal decomposition of hydride present in the compact to release hydrogen gas to accelerate release of hydrogen from the compact.
|
申请公布号 |
US7138019(B2) |
申请公布日期 |
2006.11.21 |
申请号 |
US20040900017 |
申请日期 |
2004.07.26 |
申请人 |
TDK CORPORATION |
发明人 |
TOKORO SEIGO;TOMIZAWA SHIRO;MORI TERUO |
分类号 |
H01F1/08;B22F3/00;B22F3/10;H01F1/055;H01F1/22;H01F41/02;H01L41/22 |
主分类号 |
H01F1/08 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|