摘要 |
PROBLEM TO BE SOLVED: To provide a method of repairing splines and seal teeth (20) of a claw component (10). SOLUTION: The method included performing a low energy input weld to deposit repair material (50) on the non-worn, non-pressure face (34) of the splines (20) while minimizing a grain size at HAZ. Then, the splined area (12) of the component (10) is machined to the original spline contour by removing original material and the excess repair material (50) from the worn pressure face (40) of the splines (20). In this way, the claw component provided with splines (20'), which have original component material and are rearranged radially clockwise, is formed on the pressure face (40') of the teeth (20'). COPYRIGHT: (C)2007,JPO&INPIT |