摘要 |
PROBLEM TO BE SOLVED: To provide a carbonated inorganic cured body of high texture stability that can be produced by low-temperature carbonation treatment in a short time. SOLUTION: In this method of producing a carbonated inorganic cured body, wollastonite that has <=1 μm of 10% cumulation diameter in the grain size volume distribution and >=1 m2/g of nitrogen adsorption specific surface area is mixed with water, formed and the formed product is subjected to the carbonation treatment at 30-200 deg.C under the conditions of the atmospheric pressure (0 MPa)-20 MPa. |