摘要 |
An improved bipolar plate stainless steel alloy comprises, in weight percent, about 20% to about 30% chromium, about 10% to about 25% nickel, about 1% to about 9 % molybdenum, and up to about 4% copper, where the weight percentage of chromium plus nickel plus molybdenum is greater than about 51 percent. The weight percentage of chromium plus molybdenum may be greater than about 1.66 times the weight percentage of nickel. In addition, the ratio of chromium equivalents to nickel equivalents may be greater than about 1.66.
|