摘要 PROBLEM TO BE SOLVED: To obtain high pickling efficiency at a low cost in the case the ferritic heat resisting steel sheet is pickled by using mixed acids of a pickling accelerator containing sulfuric acid and mercapto group. SOLUTION: The amount of precipitated P is specified to≥0.017% in pickling the ferritic heat resisting steel sheet containing, by mass, 0.0015 to 0.0080% C, 0.05 to 0.70% Si, 0.05 to 0.70% Mn, 0.017 to 0.035% P, 0.005 to 0.0010% S, 10.5 to 18.0% Cr, 0.001 to 0.050% Mo, 0.001 to 010% Cu, 0.0040 to 0.150% N, 10+(C+N)+2xP to 0.30% Ti, and the balance consisting of Fe and inevitable impurities by the mixed acids prepared by adding mercaptoacetic acid to sulfuric acid. COPYRIGHT: (C)2006,JPO&NCIPI
申请公布号 JP2005298911(A) 申请公布日期 2005.10.27
申请号 JP20040117511 申请日期 2004.04.13
申请人 NIPPON STEEL & SUMIKIN STAINLESS STEEL CORP 发明人 TERAOKA SHINICHI;SAKAMOTO TOSHIHARU;FUTAKA MIKIO;IIDA HIDENORI
分类号 C21D8/02;C22C38/00;C22C38/28;C23G1/08;(IPC1-7):C23G1/08 主分类号 C21D8/02
代理机构 代理人
主权项
地址