摘要 |
FIELD: road-transport industry. ^ SUBSTANCE: method includes applying substance on asphalt-concrete mixture. As substance silicon-organic modifier is used, loss of which at 1 m2 of area of pre-placed on road asphalt-concrete mixture at temperature 80-100°C is no less than 0,3-0,5 kg. After applying modifier, asphalt-concrete mixture is rolled. ^ EFFECT: higher efficiency, no corrosive effect on metals, effective at temperature above -20°C. ^ 2 cl, 3 tbl, 3 ex, 1 dwg |