发明名称 Aluminous metal article
摘要 Aluminium alloys suitable for anodic oxidation comprise:- .Al. .Mg 0.4 -2.0%,.preferably 0.6-1.0% .Cu 0.05-0.15%. .Cr 0.05-0.15%. .Fe up to 0.15%,.preferably up to 0.08% max .Si up to 0.15%,.preferably up to 0.06% max .Mn up to 0.05%,.preferably up to 0.01% max .Ti trace to 0.05%,.preferably up to 0.02% max Prior to anodic treatment the alloy may be soaked at 1100 DEG to 1150 DEG C. for 4 to 16 hours, cooled to room temperature and then reheated to hot working temperature or it may be cooled directly to the hot-working temperature after the soaking treatment.
申请公布号 GB914800(A) 申请公布日期 1963.01.02
申请号 GB19610023699 申请日期 1961.06.30
申请人 ALUMINUM COMPANY OF AMERICA 发明人
分类号 C22C21/06;C25D11/04 主分类号 C22C21/06
代理机构 代理人