摘要 <p>Method for melting highly pure, aggressive or high melting point glass in a skull crucible (1) comprises heating the melt with a coil (1.3) surrounding it. The molten glass is poured off above the coil and insoluble components are retained in the crucible by a cooled bridge (2) which dips into the melt. An Independent claim is included for apparatus for carrying out the method with a glass outlet (1.5) in the crucible above the top of the coil.</p>
申请公布号 JP2005504707(A) 申请公布日期 2005.02.17
申请号 JP20030534345 申请日期 2002.10.01
申请人 发明人
分类号 H05B6/24;C03B1/02;C03B3/00;C03B5/02;C03B5/18;C03B5/187;C03B5/193;C03B5/235;F27D11/06;H05B6/34;H05B6/36;(IPC1-7):C03B5/235 主分类号 H05B6/24