PROCESS FOR RECOVERY OF NICKEL AND COBALT BY HEAP LEACHING OF LOW GRADE NICKEL OR COBALT CONTAINING MATERIAL |
摘要 |
<p>A process for the recovery of nickel and cobalt from laterite ores, the process including the steps of: a) beneficiating the ore to separate it into a beneficiated upgraded ore fraction and a coarse, siliceous low grade rejects fraction which is substantially free from fines and clay materials; b) separately processing the upgraded ore fraction for the recovery of nickel and cobalt; and c) subjecting the low grade rejects fraction to a heap leach process with an acid supplemented solution to create a heap leachate for further nickel and cobalt recovery processing.</p> |
申请公布号 |
WO2005005671(A1) |
申请公布日期 |
2005.01.20 |
申请号 |
WO2004AU00943 |
申请日期 |
2004.07.13 |
申请人 |
BHP BILLITON SSM TECHNOLOGY PTY LTD;MILLER, GEOFFREY, WILLIAM;LIU, HOUYUAN |
发明人 |
MILLER, GEOFFREY, WILLIAM;LIU, HOUYUAN |
分类号 |
C22B3/08;B03B5/00;B03B7/00;C22B3/04;C22B3/06;C22B3/10;C22B23/00;(IPC1-7):C22B3/06 |
主分类号 |
C22B3/08 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|