摘要 |
PROBLEM TO BE SOLVED: To provide a sheet pallet having an increased coefficient of friction without losing rigidity. SOLUTION: The sheet pallet (1) includes a main layer (2) made of a propylene-based polymer and front layers (3 and 4) laminated on one or both of surfaces of the main layer. The front layer is formed of a composition consisting of (A) a propylene-based polymer of 0-95wt.%, (B) an ethylene (co)polymer of 5-100 wt.% obtained by (co)polymerizing an ethylene or ethylene with 3-20Cα-olefin under the existence of a IV-group transition metal compound containing ligand having a cyclopentadienyl skeleton and having a density of 0.86-0.97 g/cm<SP>3</SP>, a melt flow rate of 0.01-50 g/10 min, a molecular weight distribution parameter of Mw/Mn ranging from 1.8 to 3.5, and a composition distribution parameter of Cb1.2 or less, and (C) an ethylene-based polymer of 0-45 wt.% (where the total of components (A), (B) and (C) is 100 wt.%). COPYRIGHT: (C)2005,JPO&NCIPI
|