发明名称 Cu-Ni-Si ALLOY AND ITS PRODUCTION METHOD
摘要 PROBLEM TO BE SOLVED: To provide a Cu-Ni-Si alloy for an electronic material in which high strength and high electrical conductivity are made compatible. SOLUTION: In the Cu-Ni-Si alloy having a composition comprising, by mass, 1.0 to 4.5% Ni and 0.25 to 1.5% Si, and the balance Cu with inevitable impurities, provided that each mass concentration of Ni and Si is defined as [Ni] and [Si], the mass concentration ratio between Ni and Si, [Ni]/[Si] is 4 to 6, and also,χdefined by formula (1) is 0.1 to 0.45: ([Ni]-4χ)<SP>2</SP>([Si]-χ)=1/8 (formula 1). COPYRIGHT: (C)2005,JPO&NCIPI
申请公布号 JP2004315940(A) 申请公布日期 2004.11.11
申请号 JP20030114689 申请日期 2003.04.18
申请人 NIKKO METAL MANUFACTURING CO LTD 发明人 ISHIKAWA HIROYASU;NIIMI HISAHIRO;HATANO TAKATSUGU
分类号 C22C9/06;(IPC1-7):C22C9/06 主分类号 C22C9/06