发明名称 |
COMPOSITE SINTERED COMPACT, AND PRODUCTION METHOD THEREFOR |
摘要 |
PROBLEM TO BE SOLVED: To sufficiently improve the joining strength of a composite sintered compact by suppressing the peeling of boundaries caused by sintering shrinkage generated only in either member side in the initial stage of sintering. SOLUTION: The composite sintered compact consists of a first member 10 obtained by sintering first raw material powder consisting mainly of first metal powder 1 and a second member 20 obtained by sintering second raw material powder consisting mainly of second metal powder 2 having a sintering starting temperature higher than that of the first metal powder 1, and both members are integrally joined by sintering. The first metal powder 1 is incorporated into the second member 20 within a range of such a blending amount that the properties of the second member 20 to be required can be secured. COPYRIGHT: (C)2005,JPO&NCIPI
|
申请公布号 |
JP2004292878(A) |
申请公布日期 |
2004.10.21 |
申请号 |
JP20030085731 |
申请日期 |
2003.03.26 |
申请人 |
AISIN SEIKI CO LTD |
发明人 |
TAKAYAMA TOSHIHIKO;KURITA NOBUAKI |
分类号 |
B22F7/06;B22F3/10;(IPC1-7):B22F7/06 |
主分类号 |
B22F7/06 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|