发明名称 SYNTHESIS METHOD FOR SWELLING Na-4-mica
摘要 <p>Disclosed herein is the synthesis method for swelling Na-4-mica comprising a step of thermally treating mixture of Si source, Al source, MgF2 and NaCl with the molar compositions of 1~2 (based on the Si atom): 1~2 (based on the Al atom): 2~4: 2~6 at the temperature of 600~1000 °C for 0.5~72 hours. According to the present invention, it is possible to repress the formation of impurities and eliminate tedious postpreparation of the conventional method. In addition, the crystal size of Na-4-mica could be manipulated by changing initial molar ratio of Al source material/NaCl.</p>
申请公布号 WO2004048267(A1) 申请公布日期 2004.06.10
申请号 WO2002KR02227 申请日期 2002.11.27
申请人 PARK, MAN;CHOI, CHOONG-LYREAL;LEE, DONG-HOON;CHOI, JYUNG;KIM, KWANG, SEOP;KIM, SANGSOO 发明人 PARK, MAN;CHOI, CHOONG-LYREAL;LEE, DONG-HOON;CHOI, JYUNG;KIM, KWANG, SEOP;KIM, SANGSOO
分类号 C01B33/38;(IPC1-7):C01B33/38 主分类号 C01B33/38
代理机构 代理人
主权项
地址