摘要 |
The present invention provides a copolyester resin composition which has good physical properties, biodegradability and processability and a process for preparing and/or producing the same. To improve the biodegradability and physical properties of the copolyester, the present invention applied multi-stage reaction step, and copolyester resin having number average molecular weight of from 30,000 to 70,000, weight average molecular weight of from 100,000 to 600,000, melting point of from 55° C. to 120° C., and melt index of from 0.1 to 30 g/10 minute (190° C., 2,160 g) is obtained. The processability and physical properties of the copolyester resin of the present invention has been greatly enhanced by incorporating (i) an "aromatic-aliphatic prepolymers" having number average molecular weight of from 300 to 30,000 and the contiguous repeating unit of aromatic group in the dicarboxylic acid position of "aromatic-aliphatic prepolymers" is less than 5. Thus it can be processed by using the conventional processing equipment for polyethylene and polypropylene without any modification.
|