发明名称 Process for oxidizing iron-doped lithium niobate
摘要 A process for oxidizing iron ions contained within iron-doped lithium niobate. The process comprises the steps of protonating the iron-doped lithium niobate crystal and then placing the same into a pressure chamber where between 10-100 atmospheres of dry, ultra-pure pressurized oxygen are applied. While under pressure, the crystal is heated to approximately 950° C. at a rate not to exceed 50° C. per minute, and preferably at a rate not less than 25° C. per minute. The resulting lithium niobate crystal will thereafter contain iron ions wherein the divalent iron ion ratio to the trivalent iron ion ratio is approximately 1:100.
申请公布号 US6652780(B2) 申请公布日期 2003.11.25
申请号 US20020092137 申请日期 2002.03.06
申请人 NORTHROP GRUMMAN 发明人 STOLL HAROLD M
分类号 C30B33/00;G03H1/02;G11B7/0065;G11B7/26;(IPC1-7):G02B5/20;C01P1/02 主分类号 C30B33/00