摘要 |
<p><P>PROBLEM TO BE SOLVED: To prepare a thermoplastic resin sheet having excellent impact strength, transparency and rigidity and improved balance among other physical properties. <P>SOLUTION: This thermoplastic resin sheet is obtained by molding a resin composition comprising (A) 5-85 mass % of a copolymer composed of 70-95 mass % of an aromatic vinyl monomer unit and 5-30 mass % of a conjugated diene unit, (B) 5-85 mass % of a copolymer composed of 70-85 mass % of the aromatic vinyl monomer unit and 15-30 mass % of a (meth)acrylic acid ester- based monomer unit and (C) 1-30 mass % of a copolymer composed of 20-60 mass % of the aromatic vinyl monomer unit and 40-80 mass % of the conjugated diene unit. <P>COPYRIGHT: (C)2004,JPO</p> |