摘要 |
A method for the manufacture of a plastic window comprising a frame (2) and at least one pane (4a, 4b) of transparent plastic, in which method the pane (4a, 4b) is joined with the frame (2) at an abutment surface (3a, 3b) provided thereon. The joining is performed by welding with laser light (8), and while the welding is performed, an average abutment pressure of at least approx. 2 MPa is provided between the pane (4a, 4b) and the frame (2). <IMAGE> |