发明名称 METHOD FOR PREPARING HYDROGENATION PURIFICATION CATALYST
摘要 A method is used to produce a hydrorefining catalyst containing an inorganic oxide carrier and a hydrogenation-active metal in which pores having pore diameters of not more than 50 nm have a pore volume of not less than 0.4 cm3/g, pores having pore diameters of not less than 50 nm have a pore volume of not less than 0.2 cm3/g, and pores having pore diameters of not less than 1000 nm have a pore volume of not more than 0.1 cm3/g. The method comprises the steps of mixing and forming a pseudo-boehmite powder which has a phase transition temperature to .alpha.-alumina of 1220 to 1240 °C; and calcinating the formed pseudo-boehmite under a condition in which the pseudo-boehmite is converted into .gamma.-alumina.
申请公布号 CA2727654(A1) 申请公布日期 2003.08.14
申请号 CA20032727654 申请日期 2003.02.05
申请人 JX NIPPON OIL & ENERGY CORPORATION 发明人 SAITO, TORU;NAKAOKA, CHIKANORI
分类号 B01J37/08;B01J21/04;B01J23/28;B01J27/19;B01J35/10;B01J37/04;C10G45/04;C10G45/08;C10G45/12 主分类号 B01J37/08