发明名称 METHOD FOR PREPARING PURE MAGNESIUM OXIDE
摘要 FIELD: inorganic chemistry, chemical technology. SUBSTANCE: natural serpentinite is ground to particles size 0.5 mm, not above, dissolved in H2SO4, H2O2 is added and cooled. Crystallized mixture is washed out with water to MgSO4 concentration 290-330 g/l and unsolved residue is separated from prepared sulfate solution. Then NaOH solution with concentration 40-50% is added to filtrate to pH = 5-7. Compounds of impurity metals are precipitated as hydroxides. Precipitate is separated, NaOH solution with concentration 40-50% is added to filtrate to pH = 10-12, heated to 30-40 C, prepared precipitate Mg(OH)2 is filtered off and washed out with water up to MgSO4 content in washing out waters 0.5-4 g/l. Washed out product is dried at 350-400 C to moisture 2%, not above, and subjected for thermal treatment at 800-850 C for 40 min to yield magnesium oxide. Finally, magnesium oxide is washed with water and filtered off. Magnesium oxide comprises, wt.-%: MgO, 97, not less; Fe, 0.100-0.254; MnO, 0.059-0.14; total impurity of other metal oxides, the balance. EFFECT: improved preparing method. 3 ex
申请公布号 RU2209780(C2) 申请公布日期 2003.08.10
申请号 RU20000126921 申请日期 2000.10.26
申请人 ALEKSANDROV JURIJ JUR'EVICH;PARAMONOV GENNADIJ PETROVICH;OLEJNIKOV JURIJ VASIL'EVICH 发明人 ALEKSANDROV JU.JU.;PARAMONOV G.P.;OLEJNIKOV JU.V.
分类号 C02F5/02 主分类号 C02F5/02
代理机构 代理人
主权项
地址