摘要 A turbine rotor material, that has sufficient corrosion resistance and stress corrosion cracking resistance and appropriate strength and toughness in a good balance, and a manufacturing method thereof are provided. The turbine rotor material is a 12Cr alloy steel that contains: C of 0.01 to 0.10%, Si of 0.01 to 0.50%, Mn of 0.1 to 1.0%, Cr of 9 to 13%, Ni of 2 to 7%, Mo of 0.3 to 3%, N of 0.01 to 0.10%, all in weight percent, and remains of Fe and incidental impurities.
申请公布号 US2003145916(A1) 申请公布日期 2003.08.07
申请号 US20020280052 申请日期 2002.10.25
申请人 KAMADA MASATOMO;SAITO MASAHIRO;FUJITA AKITSUGU;TAKANO YUSAKU 发明人 KAMADA MASATOMO;SAITO MASAHIRO;FUJITA AKITSUGU;TAKANO YUSAKU
分类号 F01D5/02;C21D1/18;C21D6/00;C22C38/00;C22C38/44;C22C38/54;C22C38/60;F01D5/28;(IPC1-7):C21D1/18 主分类号 F01D5/02