发明名称 Outer race for constant velocity joint, having improved anti-flaking properties and shaft strength, and process for producing the same
摘要 Disclosed are an outer race for a constant velocity joint, having improved anti-flaking properties and shaft strength, and a process for producing the same. The outer race for a constant velocity joint includes a cup and a serration and comprises by weight carbon: 0.45 to 0.59%, silicon: 0.15 to 0.4%, manganese: 0.15 to 0.45%, sulfur: 0.005 to 0.15%, molybdenum: 0.1 to 0.35%, boron: 0.0005 to 0.005%, aluminum: 0.015 to 0.05%, and titanium: 0.015 to 0.03%, the proportion of the effective case depth in track grooves of the cup being 0.25 to 0.45 in terms of the ratio of the effective case depth t to the wall thickness of the cup w, t/w, the proportion of the effective case depth of the involute serration in its end being 0.20 to 0.50 in terms of the ratio of the effective case depth t to the radius r, t/r. The involute serration in its end preferably has a former austenite grain size of not less than 8 in terms of the grain size number specified in JIS (Japanese Industrial Standards).
申请公布号 US6602358(B1) 申请公布日期 2003.08.05
申请号 US19990442490 申请日期 1999.11.18
申请人 NIPPON STEEL CORPORATION;HONDA MOTOR CO., LTD. 发明人 OCHI TATSURO;KANISAWA HIDEO;NAITO KENICHIRO;TAMURA JOJI;SAGA MASAYOSHI
分类号 F16D3/20;C21D1/10;C21D9/00;C21D9/40;C22C38/12;C22C38/14;C22C38/60;F16D3/223;(IPC1-7):C22C38/14 主分类号 F16D3/20
代理机构 代理人
主权项
地址
您可能感兴趣的专利