发明名称 |
METHOD FOR PRODUCING COATING MATERIAL COMPOSITION |
摘要 |
PROBLEM TO BE SOLVED: To obtain a coating material composition free from the formation of a residue layer on the coating film surface even after the immersion over a long period, resistant to the generation of defects such as crack and peel of the coating film, dissipating the coating film at a constant rate higher than a specific level to reduce the residue layer, exhibiting the performance to prevent the adhesion of marine life over a long period and having good recoatability and marine life adhesion preventing performance corresponding to the rigging period. SOLUTION: A method for the production of the coating material composition comprises the mixing and dispersion of (A) a rosin compound composed of a rosin or a rosin derivative, (B) a polymer containing an organic silyl ester group and composed of a homopolymer or a copolymer of a monomer M having a triorganosilyl group wherein at least one of the three alkyl or aryl groups (R<SP>1</SP>to R<SP>3</SP>) is a≥3C group or a copolymer of the monomer M and other polymerizable monomers and (C) an antifouling agent composed of an inorganic compound or a metal-containing organic compound. COPYRIGHT: (C)2003,JPO
|
申请公布号 |
JP2003176443(A) |
申请公布日期 |
2003.06.24 |
申请号 |
JP20020381833 |
申请日期 |
2002.12.27 |
申请人 |
NIPPON YUSHI BASF COATINGS KK;NITTO KASEI CO LTD |
发明人 |
ITO MASAYASU;FUKUDA SHIGEO;KAWAKAMI YOSHIHISA;MATSUBARA YOSHIRO;KAWAMURA YASUSHI;MASUOKA SHIGERU;HONDA YOSHIHIRO |
分类号 |
C09D143/04;C09D5/16;C09D193/04;(IPC1-7):C09D143/04 |
主分类号 |
C09D143/04 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|