摘要 |
Processes for producing gray cast iron and the resulting gray cast iron exhibiting consistently good surface finish with prolonged tool life during finish machining with cubic boron nitride and silicon nitride cutting tools at high cutting speeds and low feed rates are provided comprising (1) adding microalloying elements with strong affinity for nitrogen to a gray iron melt; (2) adding microalloying elements with strong affinity for carbon to said melt; and (3) adding microalloying elements with strong affinity for oxygen to said melt, to form a chemically stable, high melting or refractory oxide protective layer at the cutting edge of the tool during metal cutting, thereby suppressing chemical wear.
|