<p>An article includes an antireflection composite material, a substrate, and an inorganic layer deposited onto the substrate. The inorganic layer has a thickness of from about 1 nm to about 10 nm. The article includes a polymer layer in contact with the inorganic layer to form an outer surface of the antireflection composite material. The polymer layer has a thickness of from about 70 nm to about 120 nm.</PTEXT></p>