A melt-processable fluorine-containing polymer is melt kneaded with a kneader which has a residence time of at least 10 minutes, a usable volume ratio (usable space in a container/space in a container) of larger than 0.3, and a power factor K of less than 8000, the power factor K being represented by the formula: K = Pv/ mu /n<2> in which Pv is a power requirement per unit volume (W/m<3>), mu is a melt viscosity (Pa.s), and n is a rotation speed (rps), to effectively remove terminal groups and bonds in the backbones, which are unstable during melt kneading, from the melt-processable fluorine-containing polymer, and obtain a colorless fluorine-containing polymer. |