发明名称 PROCESS FOR PRODUCTION OF THERMOPLASTIC ELASTOMER COMPOSITION
摘要 <p>A process for production of a thermoplastic elastomer composition by melt-kneading a mixture in one step to thereby conduct dynamic crosslinking, wherein the mixture comprises a hydrogenated block copolymer (a1) which is prepared by hydrogenating a block copolymer comprising a vinyl aromatic polymer block (A1) and a conjugated diene polymer block (B1) and has a number-average molecular weight of 200000 or above and, if necessary, a nonhydrogenated block copolymer (a2) comprising a vinyl aromatic polymer block (A2) and a conjugated diene polymer block (B2), and contains a nonaromatic rubber softener (b), a peroxide-crosslinkable olefin resin (c) having a density of 0.94 g/cm3 or above, a peroxide-decomposable olefin resin (d), an organic peroxide (e), and a crosslinking aid (f), the amount of (b) being 50 to 250 parts by mass per 100 parts by mass of the sum of (a1) + (a2), the amount of (c) being 2.5 to 50 parts by mass per 100 parts by mass of (a); and the amount of (d) being 0.5 to 10 times that of (c) by mass.</p>
申请公布号 WO2002102895(P1) 申请公布日期 2002.12.27
申请号 JP2002005910 申请日期 2002.06.13
申请人 发明人
分类号 主分类号
代理机构 代理人
主权项
地址