发明名称 |
Process for making a work piece having a major phase of alpha from a titanium alloy |
摘要 |
Quenching a work piece made of a titanium alloy having a temperature higher than 800 C. to a temperature lower than 500 C. at a cooling rate greater than 10 C./second between 800 C. and 500 C. is used to render the cooled work piece containing alpha'' phase as a major phase. The work piece is preferably a medical implant
|
申请公布号 |
US2002179208(A1) |
申请公布日期 |
2002.12.05 |
申请号 |
US20020157121 |
申请日期 |
2002.05.30 |
申请人 |
JIIN-HUEY CHERN LIN |
发明人 |
LIN JIIN-HUEY CHERN;JU CHIEN-PING;LEE CHIH-MIN;HO WEN-FU;LIN DAN JAE;CHENG WEN-WEI;LIN CHIA WEI;YANG CHE CHIN |
分类号 |
A61L27/06;C22C14/00;(IPC1-7):C22F1/18 |
主分类号 |
A61L27/06 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|