Thermoplastic elastomer composition for a powder for slush molding and skin formed therefrom |
摘要 |
A thermoplastic elastomer composition for a powder material used for slush molding. The thermoplastic elastomer composition consists of a polypropylene resin and 20 to 500 parts by mass of a hydrogenated block copolymer per 100 parts by mass of the polypropylene resin. The hydrogenated block copolymer has a) at least one polymer block A with a primary component that is a vinyl aromatic hydrocarbon monomer unit and b) at least one polymer block B with a primary component that is a hydrogenated butadiene monomer unit. The polymer block B has a hydrogenation degree of at least 90%. The vinyl aromatic hydrocarbon in the hydrogenated block copolymer is present in an amount more than 5 mass % and less than 25 mass %. The polymer block B before hydrogenation contains 62 mol % or more 1,2 bonds on average. The melt flow rate (MFR) of the thermoplastic elastomer composition is at least 10 g/10 min at 230° C. under a load of 2.16 kgf in accordance with Japanese Industrial Standards (JIS) K7210.
|
申请公布号 |
US2002151649(A1) |
申请公布日期 |
2002.10.17 |
申请号 |
US20010055169 |
申请日期 |
2001.10.26 |
申请人 |
ENAMI HIROHIDE;ONO KENROU;KUBOMOTO KENJI;TODA YOSHIHIRO |
发明人 |
ENAMI HIROHIDE;ONO KENROU;KUBOMOTO KENJI;TODA YOSHIHIRO |
分类号 |
C08J3/12;B29C41/18;B29K23/00;C08J5/00;C08L5/14;C08L23/10;C08L23/12;C08L23/16;C08L25/04;C08L25/10;C08L53/02;C08L91/00;(IPC1-7):C08L53/00 |
主分类号 |
C08J3/12 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|