发明名称 High speed steel with good high temperature strength manufactured by powder metallurgy
摘要 Steel object produced by decomposing a liquid metal stream of an alloy with nitrogen to form a metal powder and compacting the powder with optional deformation comprises a chemical composition containing (in weight %) 1.51-2.5 carbon, up to 0.8 silicon, up to 1.5 manganese, 3.5-4.5 chromium, 13.3-15.3 tungsten, 2.0-3.0 molybdenum, 4.5-6.9 vanadium, 10.05-12.0 cobalt, up to 0.52 sulfur, up to 0.2 nitrogen, maximum 100 ppm oxygen, and a balance of iron. The amount of manganese minus sulfur is at least 0.19. The ratio of concentrations of tungsten to molybdenum is 52.-6.5. Preferred Features: The steel has the following composition (in weight %) 1.75-2.38 C, 0.35-0.75 Si, 0.28-0.54 Mn, 3.56-4.25 Cr, 13.90-14.95 W, 2.10-2.89 Mo, 4.65-5.95 V, 10.55-11.64 Co and 0.018-0.195 N.
申请公布号 EP1249511(A1) 申请公布日期 2002.10.16
申请号 EP20010890331 申请日期 2001.12.05
申请人 BOEHLER EDELSTAHL GMBH 发明人 MAILI, INGRID;RABITSCH, ROLAND;LIEBFAHRT, WERNER
分类号 B22F3/15;C22C33/02;C22C38/00;C22C38/22;C22C38/24;C22C38/30;C22C38/36;C22C38/60 主分类号 B22F3/15
代理机构 代理人
主权项
地址