POLYOXYMETHYLENE COPOLYMER AND MOLDED ARTICLE THEREOF
摘要
A polyoxymethylene copolymer obtained by copolymerizing trioxane with 1,3-dioxolane in a molar ratio of 100/(8-20), characterized by having the following properties: (i) the crystallization time at 143 DEG C is 10 to 2,000 seconds; (ii) the number of cycles in a folding endurance test is 30 to 1,000; and (iii) the thermal stability in residence is 40 minutes or longer. Also provided is a molded article formed from the copolymer. The polyoxymethylene copolymer is excellent in folding endurance and thermal stability and has satisfactory moldability.
申请公布号
WO02077049(A1)
申请公布日期
2002.10.03
申请号
WO2002JP02920
申请日期
2002.03.26
申请人
MITSUBISHI GAS CHEMICAL COMPANY, INC.;NAKAMURA, TAKAHIRO;FURUKAWA, MASANORI;OKAMURA, AKIRA;NAKAYA, DAIGO;MASUMOTO, ISAMU