发明名称 |
MANUFACTURING METHOD OF HOT ROLLED STEEL SHEET |
摘要 |
PROBLEM TO BE SOLVED: To provide a manufacturing method of a hot rolled steel sheet having small surface roughness of a same degree as that of a surface of grinding treated, without making grinding treatment. SOLUTION: In the manufacturing method characterized in that a light rolling draft with more than 1.8% of a rolling reduction rate is performed under non- lubricant condition and in that the light rolling draft with less than 5% of the rolling reduction rate is also performed under non-lubricant condition after acid pickling is applied to the hot-rolled steel sheet, the light rolling draft is performed by means of a roll having surface roughness of 1.0 to 4.5μm 10 point average roughness.
|
申请公布号 |
JP2002219502(A) |
申请公布日期 |
2002.08.06 |
申请号 |
JP20010018885 |
申请日期 |
2001.01.26 |
申请人 |
KAWASAKI STEEL CORP |
发明人 |
ISHIKAWA TAKASHI;TOMINAGA YOICHI;KUKIZAKI TAICHI |
分类号 |
B21B1/22;(IPC1-7):B21B1/22 |
主分类号 |
B21B1/22 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|