摘要 |
PROBLEM TO BE SOLVED: To make a fluororesin layer which has a large content of a vinylidene fluoride(VDF) unit and is excellent in fuel-barrier properties adhere well and directly to a polyamide resin layer, etc., without deteriorating the fuel-barrier properties. SOLUTION: In a bonded laminate, the fluororesin layer of a fluororesin containing at least 60 mole% of the VDF unit is made to adhere well and directly to a thermoplastic resin layer having the content of a terminal amino group of at least 4×10-5 gram equivalent/g. A fuel hose includes the bonded laminate in which the fluororesin layer is arranged as the inner layer of the hose.
|