发明名称 |
METHOD FOR BAKING STEEL PART |
摘要 |
<p>A method for baking a steel part, comprising the step of rapidly heating the surface layer part of the steel part to 100 to 300 DEG C by a high frequency or a ultra high frequency, particularly, of 10 KHz or more to produce a temperature difference between the surface layer part and the inside of the steel part so as to cause a strain in lattices in order to remove diffusive hydrogen related to hydrogen embrittlement or move the state of presence thereof to that of non-diffusive hydrogen not related to hydrogen embrittlement, whereby a delayed rupture is prevented from being produced by the diffusive hydrogen occluded by the steel parts such as screws and bolts.</p> |
申请公布号 |
WO0246479(A1) |
申请公布日期 |
2002.06.13 |
申请号 |
WO2001JP10606 |
申请日期 |
2001.12.05 |
申请人 |
AOYAMA SEISAKUSHO CO., LTD.;SUZUKI, TAKAMASA |
发明人 |
SUZUKI, TAKAMASA |
分类号 |
C21D1/10;C21D1/34;C21D3/06;C21D9/00;(IPC1-7):C21D3/06;C21D6/00 |
主分类号 |
C21D1/10 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|