LA INVENCION SE REFIERE A UNA FIBRA MINERAL POBRE EN HIERRO RESISTENTE A TEMPERATURAS ELEVADAS. LA FIBRA MINERAL TIENE LA SIGUIENTE COMPOSICION EN % EN PESO: SIO 2 35 - 45, AL SUB,2 O 3 18 - 25, TIO 2 0 - 3, MGO 12 - 20, CAO 10 - 20, NA 2 O + K 2 ) 0 - 3, HIERRO (FE 2 O 3 +FEO) 0 - 3, B 2 ) 3 0 - 3, P 2 O 5 0 - 4, OT ROS 0 - 3, SIENDO LA SUMA DE FEO + MGO 15 % EN PESO.
|