<p>A method of forming a co-axial interconnect line in a dielectric layer is provided. The method includes defining a trench in the dielectric layer and then forming a shield metallization layer within the trench. After forming the shield metallization layer, a conformal oxide layer is deposited within the shield metallization layer. A center conductor is then formed within the conformal oxide layer. Once the center conductor is formed, a fill oxide layer is deposited over the center conductor. A cap metallization layer is then formed over the fill oxide layer and is in contact with the shield metallization layer.</p> |