发明名称 PRODUCTION OF FLAKY TITANATE
摘要 PROBLEM TO BE SOLVED: To produce a flaky titanate having uniform particle size of severalμm order. SOLUTION: In this method for producing the flaky titanate expressed by a formula, AxMy(square)zTi2-(y+z), (in the formula, each of A and M represents a metal having a different valency of 1-3, (square) represents a defect part of Ti and each of (x), (y) and (z) represents a positive number satisfying respectively 0<x<1.0, 0<y+z<1.0), the objective flaky titanate is obtained by using the oxide of a metal A, M and Ti or a compound becoming the oxide by heating as raw materials and a halide or a sulfate of an alkali metal or an alkaline earth metal as a flux and firing by heating a mixture prepared by mixing to have a weight ratio flux/raw material of 0.1-2.0.
申请公布号 JP2000344520(A) 申请公布日期 2000.12.12
申请号 JP19990158086 申请日期 1999.06.04
申请人 OTSUKA CHEM CO LTD 发明人 MATSUNAGA HARUE;SUZUE MASAYOSHI