发明名称 PRECIPITATION HARDENING FERRITIC-PEARLITIC STEEL
摘要 The present invention relates to a precipitation hardening ferritic-pearlitic steel which is especially adapted for use with reciprocating valves in internal combustion engines. The steel according to the invention typically contains from 0.20 to 0.60% carbon, 0.20 to 0.95% silicon, 0.50 to 1.80% manganese, 0.004 to 0.04% nitrogen and 0.05 to 0.20% vanadium and/or niobium. The balance of the steel is comprised of iron and incidental impurities.
申请公布号 CA2018636(C) 申请公布日期 2000.10.24
申请号 CA19902018636 申请日期 1990.06.08
申请人 发明人 SCHULER, VOLKER;RICHTER, KLAUS E.
分类号 C22C38/00;C22C38/12;C22C38/38;F01L3/02;(IPC1-7):C22C38/12;C22C38/26 主分类号 C22C38/00