发明名称 |
AROMATIC POLYAMIDE FILM AND MAGNETIC RECORDING MEDIUM USING THE FILM |
摘要 |
PROBLEM TO BE SOLVED: To improve application properties by controlling the generation of wrinkles ad others in a process for forming a coated layer and a back coat layer. SOLUTION: An aromatic polyamide film has a heat distortion ratio H150 at 150 deg.C, 45 g/mm2 load of 0 to -0.08%. The absolute value of the heat distortion ratio|H100|at 100 deg.C and the absolute value of the heat distortion ratio|H150|at 150 deg.C meet formula:|H100|+|H150|<=0.1%, and the elongation of the film 1000 mm in width 10 m in length is±40 mm or below.
|
申请公布号 |
JP2000233441(A) |
申请公布日期 |
2000.08.29 |
申请号 |
JP19990037700 |
申请日期 |
1999.02.16 |
申请人 |
TORAY IND INC |
发明人 |
YONEYAMA WASUKE;ITO NOBUAKI |
分类号 |
G11B5/73;B29C55/14;B32B7/02;B32B27/34;C08J5/18;(IPC1-7):B29C55/14 |
主分类号 |
G11B5/73 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|